Polymer Property : CTE, linear = 85.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 6.00 - 85.0 µm/m-°C
3.33 - 47.2 µin/in-°F
Average value: 46.2 µm/m-°C Grade Count:33
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
CTE, linear 75.0 - 85.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
41.7 - 47.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Noryl GTX CRN500 PPE+PA6 (Asia Pacific)
Pa6 based unfilled GTX for Non-Auto marketThis data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear 80.0 - 85.0 µm/m-°C

@Temperature 0.000 - 80.0 °C
44.4 - 47.2 µin/in-°F

@Temperature 32.0 - 176 °F
ASTM D696
Styron Pulse® A20-95 PC/ABS
A medium impact strength PC/ABS blend with high heat distortion and excellent processability.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
CTE, linear 75.0 - 85.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
41.7 - 47.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL GTX GTX600 PPE+PA6 (Asia Pacific)
Pa6 based unfilled GTX
CTE, linear 75.0 - 85.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
41.7 - 47.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Noryl GTX GTX6013 PPE+PA6 (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear 75.0 - 85.0 µm/m-°C
41.7 - 47.2 µin/in-°F
Master Bond EP36AN One Part, Toughened, B-Stage Epoxy
Description: Master Bond EP36AN is a unique one component, high performance epoxy for bonding, encapsulation, potting and coating featuring thermal conductivity, electrical insulation and high tempe..