SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating at 2.0 mm. Noryl V03505 is may be an excellent material candidate for application requiring low warpage and flame resistance.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Moisture Absorption 0.0600 %
0.0600 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %
0.20 %
ISO 62
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 49 g/10 min

@Load 5.00 kg,
Temperature 300 °C
49 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Melt Index of Compound 15 g/10 min

@Load 3.80 kg,
Temperature 280 °C
15 g/10 min

@Load 8.38 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
24 g/10 min

@Load 5.00 kg,
Temperature 280 °C
24 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 147 MPa
21300 psi
ISO 2039-1
Tensile Strength at Break 50.0 MPa
7250 psi
5 mm/min; ISO 527
57.0 MPa
8270 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 50.0 MPa
7250 psi
5 mm/min; ISO 527
59.0 MPa
8560 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type I, 5 mm/min; ASTM D638
4.0 %
4.0 %
5 mm/min; ISO 527
Elongation at Yield 3.0 %
3.0 %
Type I, 5 mm/min; ASTM D638
3.0 %
3.0 %
5 mm/min; ISO 527
Tensile Modulus 4.40 GPa
638 ksi
5 mm/min; ASTM D638
5.00 GPa
725 ksi
1 mm/min; ISO 527
Flexural Strength 95.0 MPa
13800 psi
2 mm/min; ISO 178
Flexural Yield Strength 100 MPa
14500 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 4.30 GPa
624 ksi
1.3 mm/min, 50 mm span; ASTM D790
4.70 GPa
682 ksi
2 mm/min; ISO 178
Izod Impact, Notched 0.350 J/cm
0.656 ft-lb/in
ASTM D256
0.350 J/cm

@Temperature -30.0 °C
0.656 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched (ISO) 26.0 kJ/m²
12.4 ft-lb/in²
80*10*4; ISO 180/1U
24.0 kJ/m²

@Temperature -30.0 °C
11.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 3.00 J/cm²
14.3 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
3.00 J/cm²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Dart Drop, Total Energy 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 40.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
22.2 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
50.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
27.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 50.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
27.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
50.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
27.8 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
ISO 8302
Hot Ball Pressure Test <= 105 °C
<= 221 °F
IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
91.0 °C

@Thickness 3.20 mm
196 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 110 °C
230 °F
Rate B/50; ISO 306
115 °C
239 °F
Rate B/50; ASTM D1525
120 °C
248 °F
Rate A/50; ISO 306
120 °C
248 °F
Rate B/120; ISO 306
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
UL RTI, Mechanical with Impact 50.0 °C
122 °F
UL 746B
UL RTI, Mechanical without Impact 50.0 °C
122 °F
UL 746B
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
UL 94
V-0

@Thickness 2.00 mm
V-0

@Thickness 0.0787 in
UL 94
Oxygen Index 34 %
34 %
ISO 4589
Glow Wire Test 960 °C

@Thickness 3.20 mm
1760 °F

@Thickness 0.126 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ROA; IEC 60093
Dielectric Constant 3.1

@Frequency 1.00e+6 Hz
3.1

@Frequency 1.00e+6 Hz
IEC 60250
3.2

@Frequency 50.0 - 60.0 Hz
3.2

@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
26.0 kV/mm

@Thickness 1.60 mm
660 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
33.0 kV/mm

@Thickness 0.800 mm
838 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
Dissipation Factor 0.0030

@Frequency 1.00e+6 Hz
0.0030

@Frequency 1.00e+6 Hz
IEC 60250
0.0060

@Frequency 50.0 - 60.0 Hz
0.0060

@Frequency 50.0 - 60.0 Hz
IEC 60250
Descriptive Properties Value Comments
Ball Pressure Test, 75°C +/- 2°C PASSES
IEC 60695-10-2