Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL PPO534 PPE+HIPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL PPO534 PPE+HIPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPO/PS unfilled high heat
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Water Absorption 0.030 %

@Time 86400 sec
0.030 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0060 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Rockwell R 123
123
ASTM D785
Tensile Strength, Yield 72.0 MPa
10400 psi
SABIC - Japan Method
Elongation at Break 55 %
55 %
SABIC - Japan Method
Flexural Strength 104 MPa
15100 psi
ASTM D790
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
Izod Impact, Notched 1.37 J/cm
2.57 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
27.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 160 °C

@Thickness 6.40 mm
320 °F

@Thickness 0.252 in
unannealed; ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
UL 94
Electrical Properties Metric English Comments
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Dielectric Constant 2.58

@Frequency 50.0 - 60.0 Hz
2.58

@Frequency 50.0 - 60.0 Hz
ASTM D150