Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 104 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 104 MPa
15100 psi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion L1361 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Strength 104 MPa
15100 psi
X, Y direction; Condition A; ASTM D790
Rogers Corporation TMM® TMM6 Ceramic Thermoset Polymer Composite
TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope..
Flexural Strength 104 MPa
15100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6
LNP* Konduit* PX08321 a compound based on PA6 resins containing mineral. Added features include: Thermally Conductive.
Flexural Strength 104 MPa
15100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 compound
Flexural Strength 104 MPa
15100 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP LX00430 PEEK
LNP* LUBRICOMP* LX00430 is a compound based on Pelyetheretherketone containing Proprietary Fillers. Added feature of this grade is: Wear Resistant.
Flexural Strength 104 MPa
15100 psi
ASTM D790
Techmer ES Electrablend® PC 04006 FR BK Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite..
Flexural Strength 104 MPa
15100 psi
ASTM D790
Techmer ES Electrablend® PC 04007 FR BK Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by..
Flexural Strength 104 MPa
15100 psi
ASTM D 790
SABIC Innovative Plastics Valox® TS4016 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Strength 104 MPa
15100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP SF004S PA12
LNP* Thermocomp* SF004S is a compound based on Nylon 12 containing 20% glass fiber. Added features include: Heat Stabilized, Healthcare
Flexural Strength 104 MPa
15100 psi
ASTM D790
SABIC Innovative Plastics NORYL PPO534 PPE+HIPS (Asia Pacific)
PPO/PS unfilled high heat
Flexural Strength 104 MPa
15100 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP MF004AS PP
LNP THERMOCOMP* MF004AS is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Strength 104 MPa
15100 psi
at rupture; ASTM D790
Sumitomo Bakelite North America E 16521A Electrical Encapsulation Grade Epoxy
E-16521A is an encapsulation grade epoxy molding compound suitable for electrical applications such as coils.Information provided by Sumitomo Bak North America, Inc.
Flexural Strength 104 MPa
15100 psi
ASTM D790
Chase Plastics CP Pryme® N320GL (COND, 50% RH) Nylon 6 (Utility Grade), 20% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
Flexural Strength 104 MPa
15100 psi
ISO 178
Unitika TERRAMAC TE-8300 Polylactic Acid (PLA)
High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
Flexural Strength 104 MPa
15100 psi
ISO 178
Azdel Plus C321-B01 32% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C321-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope..
Flexural Strength 104 MPa
15100 psi
ISO 178
BASF Ultradur® S 4090 GM11 5/5% Glass/Mineral Filled PBT
Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber/mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventilation gri..
Flexural Strength 104 MPa
15100 psi
Method 1, 0.05"/min; ASTM D790
Proto3000 PC Fused Deposition Modeling Polymer
Description: A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating ..
Flexural Strength 104 MPa
15100 psi
ISO 178
Polyplastics Duracon® GB-25 Acetal Co-polymer (POM), Low warpage, GB 25% filling
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..