Material Notes:
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing 50% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structural.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
1.35 g/cc
0.0488 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0013 cm/cm

@Time 86400 sec
0.0013 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0028 cm/cm

@Time 86400 sec
0.0028 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 131 MPa
19000 psi
ASTM D638
141 MPa
20500 psi
ISO 527
Elongation at Break 1.7 %
1.7 %
ISO 527
1.8 %
1.8 %
ASTM D638
Tensile Modulus 10.44 GPa
1514 ksi
50 mm/min; ASTM D638
13.87 GPa
2012 ksi
1 mm/min; ISO 527
Flexural Strength 187 MPa
27100 psi
ASTM D790
214 MPa
31000 psi
ISO 178
Flexural Modulus 9.34 GPa
1350 ksi
ASTM D790
11.14 GPa
1616 ksi
ISO 178
Izod Impact, Notched 2.08 J/cm
3.90 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 66.0 kJ/m²
31.4 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 13.0 J
9.59 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 33.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
33.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 45.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
45.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 134 °C
273 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
157 °C

@Thickness 3.20 mm
315 °F

@Thickness 0.126 in
unannealed; ASTM D648