Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 25.4 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 45.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON MV00AS PP (Asia Pacific)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
CTE, linear, Transverse to Flow 45.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON MV00AS PP (Asia Pacific)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
CTE, linear, Transverse to Flow 45.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Verton MX03017 PP (Europe-Africa-Middle East)
LNP* VERTON* MX03017 is a compound based on Polypropylene resin containing Glass Fiber, Long Glass Fiber. Added features of this material include: Chemically Coupled.This data was supplied by SABIC..
CTE, linear, Transverse to Flow 45.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP OF006A PPS - Branched
LNP* THERMOCOMP* OF006A is a compound based on PPS - Branched resin containing 30% Glass Fiber.
CTE, linear, Transverse to Flow 45.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON MV00ASXP PP (Europe-Africa-Middle East)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
CTE, linear, Transverse to Flow 45.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON MV00ASXP PP (Europe-Africa-Middle East)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
CTE, linear, Transverse to Flow 45.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON MV00AS PP
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing 50% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, Structural.
CTE, linear, Transverse to Flow 45.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON MV00AS PP
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing 50% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, Structural.
CTE, linear, Transverse to Flow 45.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON MV00ASU PP
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing 50% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur..
CTE, linear, Transverse to Flow 45.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON MV00ASU PP
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing 50% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur..
CTE, linear, Transverse to Flow 45.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON MV00ASU PP (Asia Pacific)
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
CTE, linear, Transverse to Flow 45.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON MV00ASU PP (Asia Pacific)
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
CTE, linear, Transverse to Flow 45.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON MV00ASU PP (Europe-Africa-Middle East)
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
CTE, linear, Transverse to Flow 45.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON MV00ASU PP (Europe-Africa-Middle East)
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.