Polymer Property : Impact Test = 13.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Lubricomp GL004 PSU (Asia Pacific)
LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacifi..
Impact Test 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem 2210K PEI (Europe-Africa-Middle East)
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 13.0 J
9.59 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP HX03408 PA11
LNP* Thermocomp* HX03408 is a compound based on Nylon 11 containing Proprietary Fillers. Added feature includes: Clean Compound System
Impact Test 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66
LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b..
Impact Test 13.0 J
9.59 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP YH0235AC PE
LNP* Thermocomp* YH0235AC is a compound based on Polyester Elastomer containing a metal filler.
Impact Test 13.0 J
9.59 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON MV00AS PP (Asia Pacific)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Impact Test 13.0 J
9.59 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP Verton MX03017 PP (Europe-Africa-Middle East)
LNP* VERTON* MX03017 is a compound based on Polypropylene resin containing Glass Fiber, Long Glass Fiber. Added features of this material include: Chemically Coupled.This data was supplied by SABIC..
Impact Test 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Verton MX03017 PP (Europe-Africa-Middle East)
LNP* VERTON* MX03017 is a compound based on Polypropylene resin containing Glass Fiber, Long Glass Fiber. Added features of this material include: Chemically Coupled.This data was supplied by SABIC..
Impact Test 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Thermocomp SF006S PA 12
LNP* Thermocomp* SF006S is a compound based on Nylon 12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re..
Impact Test 13.0 J
9.59 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON MV00ASXP PP (Europe-Africa-Middle East)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Impact Test 13.0 J
9.59 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON MX02795 PP
LNP* VERTON* MX02795 is a compound based on Polypropylene resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, UV Stabilized, Structural.
Impact Test 13.0 J
9.59 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Europe-Africa-Middle East)
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
Impact Test 13.0 J
9.59 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON MV00AS PP
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing 50% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, Structural.
Impact Test 13.0 J
9.59 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP Verton UX06451 BK8-312 PPA
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Impact Test 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Lubricomp GL004 PSU
LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas re..
Impact Test 13.0 J
9.59 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON MV00ASU PP
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing 50% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur..
Impact Test 13.0 J
9.59 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON MV00ASU PP (Asia Pacific)
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Impact Test 13.0 J
9.59 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON MV00ASU PP (Europe-Africa-Middle East)
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Impact Test 13.0 J
9.59 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Asia Pacific)
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.