Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON MV008 PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* VERTON* MV008 is a compound based on Polypropylene resin containing Long Glass. Added features include Chemically Coupled.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 120 MPa
17400 psi
5 mm/min; ISO 527
Elongation at Break 2.0 %
2.0 %
5 mm/min; ISO 527
2.3 %
2.3 %
Flexural Strain, break, 2 mm/min; ISO 178
Tensile Modulus 9.70 GPa
1410 ksi
1 mm/min; ISO 527
Flexural Yield Strength 175 MPa
25400 psi
2 mm/min; ISO 178
Flexural Modulus 8.60 GPa
1250 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 18.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
10.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature 23.0 - 60.0 °C
66.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af