Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 8.60 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 8.60 GPa
1250 ksi
Plastcom SLOVAMID 66 GF 30 FRG 5 PA66, 30% glass fibre, flame retarder
FeaturesPA 66 for injection moulding, chemically reinforced with 30 % glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 /0,8 mm/ in accordance with ..
Flexural Modulus 8.60 GPa
1250 ksi
STN EN ISO 178
Plastcom SLOVAMID® 6 GF 30 AS PA6 reinforced with glass fiber, anti-static agent
PA 6 for injection molding, reinforced with 30% glass fiber, contains antistatic agent for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric..
Flexural Modulus 8.60 GPa
1250 ksi
ISO 178
Radici Radilon® A GV H0 30P Nylon 66-GF30
Automotive cooling liquid resistant PA66-GF30 grade designed to resist even in more severe operating condition. Indicated as "top of the class" material.Information provided by Radici group.
Flexural Modulus 8.60 GPa
1250 ksi
ISO 178, ASTM D790
Nilit Nilamid B G6 FR C4 30% Glass Fiber Reinforced, Flame Retardant PA6
Description: Nilamid B G6 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ..
Flexural Modulus 8.60 GPa
1250 ksi
ISO 178
DSM Akulon® K-FG6 (Dry) 30% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Flexural Modulus 8.60 GPa
1250 ksi
ISO 178
DSM Akulon® K-FHG6 (Dry) 30% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Flexural Modulus 8.60 GPa
1250 ksi
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 130 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified
PA 6, 30% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Flexural Modulus 8.60 GPa
1250 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON RFD04 PA 66
LNP STAT-KON* RFD04 is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 8.60 GPa
1250 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK (Asia Pacific)
LNP* Thermocomp* LF005 is a compound based on Polyetheretherketone resin containing Glass Fiber.
Flexural Modulus 8.60 GPa
1250 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON MV008 PP (Europe-Africa-Middle East)
LNP* VERTON* MV008 is a compound based on Polypropylene resin containing Long Glass. Added features include Chemically Coupled.
Flexural Modulus 8.60 GPa
1250 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
Flexural Modulus 8.60 GPa
1250 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc..
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Plenco 00755 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755..
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Plenco 2311 Phenolic, Granular, Compression Molded
PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr..
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Plenco 4349 Phenolic, Granular, Injection Molded
PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer ..
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Plenco 4527 Phenolic, Granular, Injection Molded
PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under..
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Plenco 7507 Phenolic, Granular, Compression Molded
PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut..
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Plenco 7507 Phenolic, Granular, Transfer Molded
PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut..
Flexural Modulus 8.60 GPa
1250 ksi
ISO 178-93
Wellman Wellamid® GF1398-BK1 Nylon 66, 30% Glass Fiber Reinforced
All information provided by Wellman Engineered Resins.
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Plenco 4309 Phenolic, Nodular, Injection Molded
PLENCO 04309 is a heat resistant, glass reinforced phenolic molding compound offering improved mechanical strength and electrical strength properties. UL recognized under component file E40654. 0430..
Flexural Modulus 8.60 GPa
1250 ksi
ISO 178
DSM Akulon® Ultraflow™ K-FG6 Nylon 6-30% Glass Reinforced (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Flexural Modulus 8.60 GPa
1250 ksi
ISO Data
BASF Ultradur B 4300 G6 LS BK15073 30% Glass Filled PBT
mt
Flexural Modulus 8.60 GPa
1250 ksi
ISO 178
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry)
Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
Flexural Modulus 8.60 GPa
1250 ksi
ISO 178
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry)
Ultramid B3EG6 BK00564 is a 30% glass fiber reinforced, pigmented black injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Chem Polymer Chemlon 240 G Nylon 6, 43% Glass Fiber Reinforced
A 43% glass fiber reinforced nylon 6, offering high rigidity and tensile strength, especially at high service temperatures.Data provided by the manufacturer, Chem Polymer.
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
A. Schulman ComAlloy Hiloy® 626 Nylon 6/6, Glass/Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Ashley Polymers Ashlene® PE126 PET Polyester, 30% Glass Reinforced
PET Polyester, with 30% glass reinforcement.Data provided by the manufacturer
Flexural Modulus 8.60 - 10.5 GPa
1250 - 1520 ksi
Average value: 9.44 GPa Grade Count:5
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi..
Flexural Modulus 8.60 GPa
1250 ksi
ISO 178
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry)
Ultramid B3WG6 is a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade.