Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS High flow PC+ABS material designed for local Pacific Automotive applications |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics GELOY CR3020 ASA Low-gloss ASA for profile and capstock applications |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL4019 PC (Asia Pacific) Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Asia Pacific) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX1432T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in transparent and tinted colors. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Asia Pacific) High flow PC+ABS material designed for local Pacific Automotive applications |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | ISO 180 |
Iran Petrochemical (PCC) SD-0150 Acrylonitrile Butadiene Styrene General Purpose ABS, SD 0150 grade, is a rigid thermoplastic with good processing characteristics. It is a high flow injection molding grade with considerable impact strength and medium heat deflec.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
Mitsubishi Xantar® G2F 23 R Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
Mitsubishi Xantar® MX 1094 Polycarbonate-9% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -40.0 °C |
11.9 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -40.0 °C |
11.9 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON MV008SU PP (Asia Pacific) LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Europe-Africa-Middle East) PPX7110 is an alloy of PP and PPO, providing high impact and good heat resistance. Generic identification acc. ISO11469: >PP+PPE+PS-I |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PX1180 PPE+HIPS (Europe-Africa-Middle East) Noryl* PX1180 PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is an unfilled , injection moldable grade, with improved impact performances, an ISO 306 Vicat B/120 temperature of 120 deg C and a.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | ISO 180/1A |
Borealis Daplen™ EE137AI Polypropylene Compound 10% Mineral Filled Daplen EE137AI is a 10% mineral filled grade intended for injection molding. EE137AI has been developed especially for the car industry, to be used in interior parts where high scratch resistance i.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | ISO 180 |
Polyram Polytron P50B07 Polypropylene, 50% Long Glass Fiber, UV Stabilized A chemically coupled 50% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | ISO 180 |
Polyram Polytron P50N07 Polypropylene, 50% Long Glass Fiber, UV Stabilized A chemically coupled 50% long glass fiber reinforced natural polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | ISO 179 |
Total PPC 4640 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4640 is a nucleated copolymer. PPC 4640 is characterized by good stiffness and impact resistance coupled with high creep resistance. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecolen® CP20 GR20 NL XC30 PPCP, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -40.0 °C |
11.9 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RV007ES PA 66 LNP VERTON* RV007ES is a compound based on Nylon 66 resin containing 35% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | ISO 180 |
Polyram Polytron A50B01 Nylon 6.6, 50% Long Fiber Glass 50% Long fiber glass reinforced black Nylon 6.6, heat stabilized for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa KOBLEND PCA 638F PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Similar to KOBLEND PCA 638 with an improved fluidity, suitable to mould complex items. Unfilled. Suitable for Injection Molding. Supplied as pellets.ISO dat.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -40.0 °C |
11.9 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RF-7007 EM HS PA 66 (Asia Pacific) LNP VERTON* RF-7007 EM HS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |