Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp RF0049S PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp RF0049S PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP THERMOCOMP* RF0049S is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Time 86400 sec
0.0030 - 0.0050 in/in

@Time 24.0 hour
ASTM D 955
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm

@Time 86400 sec
0.010 - 0.012 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 136 MPa
19700 psi
ASTM D 638
Elongation at Break 3.3 %
3.3 %
ASTM D 638
Flexural Strength 199 MPa
28900 psi
ASTM D 790
Flexural Modulus 7.51 GPa
1090 ksi
ASTM D 790
Izod Impact, Notched 0.850 J/cm

@Temperature 23.0 °C
1.59 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 6.78 J/cm

@Temperature 23.0 °C
12.7 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 1.69 mm
V-0

@Thickness 0.0665 in
UL 94 by SABIC-IP
Users viewing this material also viewed the following: