SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features include: Flame Retardant, Internally Lubricated.
Physical Properties Metric English Comments
Density 1.79 g/cc
0.0647 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 96.0 MPa
13900 psi
5 mm/min; ISO 527
Elongation at Break 1.4 %
1.4 %
5 mm/min; ISO 527
Tensile Modulus 11.0 GPa
1600 ksi
1 mm/min; ISO 527
Flexural Yield Strength 124 MPa
18000 psi
2 mm/min; ISO 178
Flexural Modulus 8.50 GPa
1230 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 29.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
16.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 82.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
45.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 202 °C
396 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94