Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR5210R PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR5210R PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* Lexan_WR5210R compound is a wear resistant, 7% PTFE filled material.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 21.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
21.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 53.0 MPa
7690 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 75 %
75 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 83.0 MPa
12000 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.03 GPa
294 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.81 J/cm
3.39 ft-lb/in
ASTM D256
Dart Drop, Total Energy 38.0 J
28.0 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 6.40 mm
259 °F

@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C
176 °F
UL 746B
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
UL RTI, Mechanical without Impact 80.0 °C
176 °F
UL 746B
Flammability, UL94 HB

@Thickness 1.49 mm
HB

@Thickness 0.0587 in
UL 94
Optical Properties Metric English Comments
Gloss 52 %
52 %
untextured, 60 degrees; ASTM D523
Electrical Properties Metric English Comments
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
>= 120 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min
1.00 - 3.15 in/min
UL 746A
Users viewing this material also viewed the following: