Physical Properties Metric English Comments
Melt Flow 21.5 g/10 min

@Load 2.16 kg,
Temperature 260 °C
21.5 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS
Nonbrominated, nonchlorinated FR PC+ABS with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipment, monitors, enclosures, among others.
Melt Flow 21.5 g/10 min

@Load 2.16 kg,
Temperature 260 °C
21.5 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS (Asia Pacific)
CYCOLOY C6600 is a FR PC+ABS of nonbrominated, nonchlorinated flame retardant systems with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipm..
Melt Flow 21.5 g/10 min

@Load 2.16 kg,
Temperature 260 °C
21.5 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D 1238
SABIC Innovative Plastics Cycoloy® CY5211 PC+ABS (Asia Pacific)
CY5211 is a FR PC+ABS of non-brominated, non-chlorinated flame retardant systems with balanced flow, impact and hydrolytic stability.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 21.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
21.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR5210R PC
LNP* Lubricomp* Lexan_WR5210R compound is a wear resistant, 7% PTFE filled PC.
Melt Flow 21.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
21.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR5210R PC (Asia Pacific)
Wear resistant, 7% PTFE filled PC.
Melt Flow 21.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
21.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR5210R PC (Europe-Africa-Middle East)
LNP* Lubricomp* Lexan_WR5210R compound is a wear resistant, 7% PTFE filled material.
Copyright © lookpolymers.com All Rights Reserved