SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* Lexan_FL1530 compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
Physical Properties Metric English Comments
Specific Gravity 1.56 g/cc
1.56 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.00050 - 0.0025 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0025 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0015 - 0.0035 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0035 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 113 MPa
16400 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 113 MPa
16400 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 4.0 %
4.0 %
Type I, 5 mm/min; ASTM D638
Flexural Strength 172 MPa
24900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 8.41 GPa
1220 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.17 J/cm
2.19 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.60 J/cm
10.5 ft-lb/in
ASTM D4812
Dart Drop, Total Energy 18.0 J

@Temperature 23.0 °C
13.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
14.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 50.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 135 °C

@Thickness 3.20 mm
275 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C

@Thickness 3.20 mm
264 °F

@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C
176 °F
UL 746B
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
UL RTI, Mechanical without Impact 80.0 °C
176 °F
UL 746B
Flammability, UL94 V-0

@Thickness 1.47 mm
V-0

@Thickness 0.0579 in
UL 94
Electrical Properties Metric English Comments
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
>= 120 arcs
UL 746A