Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 3303 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Flock Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 3303 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed by compression, transfer or injection molding . It is UL recognized under file E40654.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.720 g/cc
0.0260 lb/in³
ASTM D1895
Density 1.58 g/cc
0.0571 lb/in³
ASTM D792
Water Absorption 0.208 %
0.208 %
ASTM D570
Linear Mold Shrinkage 0.00289 cm/cm
0.00289 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 76
76
ASTM D785
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Elongation at Break 0.53 %
0.53 %
ASTM D638
Tensile Modulus 11.6 GPa
1680 ksi
ASTM D638
Flexural Strength 72.0 MPa
10400 psi
ASTM D790
Flexural Modulus 10.5 GPa
1520 ksi
ASTM D790
Compressive Strength 159 MPa
23100 psi
ASTM D695
Izod Impact, Notched 0.174 J/cm
0.326 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.213 J/cm²
1.01 ft-lb/in²
ASTM D256
Impact 104
104
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 205 °C
401 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 203 °C
397 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Shrinkage 0.142 %
0.142 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.80e+12 ohm-cm
1.80e+12 ohm-cm
ASTM D247
Dielectric Constant 5.1
5.1
ASTM D150
Dielectric Strength 10.6 kV/mm
269 kV/in
Step by Step; ASTM D149
15.8 kV/mm
401 kV/in
Short Time; ASTM D149
Dissipation Factor 0.045
0.045
ASTM D150
Arc Resistance 182 sec
182 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638
Users viewing this material also viewed the following: