Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica.. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1530 compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP ZP001XXP PPE+PS LNP* LUBRICOMP* ZP001XXP is a compound based on PPE+PS resin containing 5% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON CD000I PS LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DE0039 PC LNP* STAT-KON* DE0039 is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Flame Retardant. Electrically Conductive. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DF002 PC LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DF002H PC LNP THERMOCOMP* DF002H is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added feature includes: Healthcare. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DX06411H PC LNP* THERMOCOMP* DX06411H is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PF00A PA 6 (Asia Pacific) LNP THERMOCOMP* PF00A is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PF00ASXS PA 6 (Asia Pacific) LNP THERMOCOMP* PF00ASXS is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 LNP* THERMOCOMP* RF-1008 is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON NV003E PC+ABS (Asia Pacific) LNP* Verton* NV003E is a compound based on PC+ABS Blend resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM HU2410 PEI 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM HU2410 PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA11 LNP THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing 40% Glass Fiber. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF008XXH PA 66 LNP* THERMOCOMP* RF008XXH is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON NV003E PC+ABS LNP* VERTON* NV003E is a compound based on PC+ABS Blend resin containing 15% Long Glass Fiber. Added features of this material include: Easy Molding, Structural. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 (Asia Pacific) LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific) LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON RV00CES PA 66 LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 (Asia Pacific) LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s). |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL FE1740PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1740PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |