Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO Value |
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO 178 |
PolyOne Nymax™ X GMF 604 40 UV Black 148 rev 4 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Flexural Modulus | 8.44 GPa | 1220 ksi | ASTM D790 |
Plenco 4100 Phenolic, Granular, Injection Molded
(discontinued **) Two-stage Phenolic. PLENCO 04100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in appliance and .. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ASTM D790 |
Plenco Valite 759 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4759. Data provided by Plenco.VALITE 759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and p.. |
|||
Flexural Modulus | 8.43 GPa | 1220 ksi | 5 mm/min; ISO 178 |
Gromax CFG33-RN13N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced PA 66, 30% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Flexural Modulus | 8.41 GPa | 1220 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1530 compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO 178 |
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |
|||
Flexural Modulus | 8.44 GPa | 1220 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP QFN16 PA 6/10 LNP* LUBRICOMP* QFN16 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 5% MOS2. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 8.41 GPa | 1220 ksi | ASTM D790 |
Solvay Technyl® C216V30 30% Glass Filled Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Flexural Modulus | 8.41 GPa | 1220 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RFN16SXZ PA 66 LNP LUBRICOMP* RFN16SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Flexural Modulus | 8.41 GPa | 1220 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Europe-Africa-Middle East) LNP* Stat-kon* Lexan_LCF1506 is a 15% carbon fiber, 6% PTFE reinforced polycarbonate. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | |
SPS Guang Zhou POBUXâ„¢ 3001G30 Flame-retarded/GF30%-PBT Characteristic: Good flame retardance, high mechanical properties, high rigidity, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) .. |
|||
Flexural Modulus | 8.39 GPa | 1220 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EXTC8143 PC (Asia Pacific) LNP* Thermocomp* EXTC8143 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good ductility, No.. |
|||
Flexural Modulus | 8.39 GPa | 1220 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP GF006 PSU LNP THERMOCOMP* GF006 is a compound based on Polysulfone resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 8.39 GPa | 1220 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP GF006XXZ PSU LNP THERMOCOMP* GF006XXZ is a compound based on Polysulfone resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 8.39 GPa | 1220 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 8.43 GPa | 1220 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL GTX APS130 PPE+PPS (Asia Pacific) PPE+PPS GF30% |
|||
Flexural Modulus | 8.43 GPa | 1220 ksi | ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX6801 PPE+PS+PA66 (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO 178 |
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0 Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO 178 |
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, DRY Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is .. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ASTM D790 |
Plenco 3509 Phenolic, Granular, Injection Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6600 MZ 315 CP Combination Nylon 66, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO 178 |
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ASTM D790 |
Ashley Polymers Ashlene® 541-33G Nylon 66, 33% Glass Reinforced Nylon 66, 33% glass reinforced for extrusion applications.Data provided by the manufacturer |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO Data |
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Dry) Ultramid B3WGM24 BK30564 is a 30% glass/mineral filled heat stabilized injection molding PA6 grade for industrial articles having medium to high rigidity and high dimensional stability. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO Data |
BASF Ultramid® TG7S BK-102 35% Glass Filled PA6 (Dry) Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified nylon 6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushi.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ASTM D790 |
A. Schulman ComAlloy Lubrilon® 610 Nylon 6, Carbon Fiber/PTFE Reinforced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Flexural Modulus | 8.41 GPa | 1220 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Asia Pacific) 15% carbon fiber, 6% PTFE reinforced polycarbonate. |