Mechanical Properties Metric English Comments
Flexural Modulus 8.41 GPa
1220 ksi
1.3 mm/min; ASTM D790
PolyOne LubriOne™ CTX-502 Natural Polyether Imide (PEI)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Flexural Modulus 8.41 GPa
1220 ksi
ISO 178
Ravago Manufacturing Americas Hylon® N1240MGHL BK Nylon 6/6
Available in North America Filler: Glass Fiber Reinforcement -15% Filler by Weight, Mineral -25% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated, Low Warpage and Heat S..
Flexural Modulus 8.41 GPa
1220 ksi
ASTM Data
BASF Capron® GR30 30% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron GR30 is a 30% glass reinforced polyamide 6 injection molding compound. IT is also available in heat stabilized (Capron GR30 HS) and/or pigmented versions. The glass fiber reinforcement enhanc..
Flexural Modulus 8.41 GPa
1220 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC
LNP* Lubricomp* Lexan_LF1530A compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
Flexural Modulus 8.41 GPa
1220 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC (Europe-Africa-Middle East)
LNP* Lubricomp* Lexan_FL1530 compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
Flexural Modulus 8.41 GPa
1220 ksi
ASTM D790
Solvay Technyl® C216V30 30% Glass Filled Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Flexural Modulus 8.41 GPa
1220 ksi
ISO 178
Solvay Technyl® C218V30 30% Glass Filled, Heat Stabilized Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Flexural Modulus 8.41 GPa
1220 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RFN16S PA 66
LNP LUBRICOMP* RFN16S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Heat Stabilized, Wear Resistant.
Flexural Modulus 8.41 GPa
1220 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RFN16SXZ PA 66
LNP LUBRICOMP* RFN16SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Heat Stabilized, Wear Resistant.
Flexural Modulus 8.41 GPa
1220 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC
LNP* Stat-kon* Lexan_LC1500N compound is a 15% carbon fiber, 6% PTFE reinforced polycarbonate.
Flexural Modulus 8.41 GPa
1220 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Europe-Africa-Middle East)
LNP* Stat-kon* Lexan_LCF1506 is a 15% carbon fiber, 6% PTFE reinforced polycarbonate.
Flexural Modulus 8.41 GPa
1220 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DX06412H PC
LNP* THERMOCOMP* DX06412H is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Flexural Modulus 8.41 GPa
1220 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DX06412H PC (Asia Pacific)
LNP* Thermocomp* DX06412H is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Flexural Modulus 8.41 GPa
1220 ksi
ASTM D790
Ecomass® 1700TU96 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyRigidInformation provided by Technical Po..
Flexural Modulus 8.41 GPa
1220 ksi
ASTM Data
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron GR30 HS is a heat stabilized 30% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
Flexural Modulus 8.41 GPa
1220 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Asia Pacific)
15% carbon fiber, 6% PTFE reinforced polycarbonate.