Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC 324CN Linear Low Density Polyethylene for Wire & Cable

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer SABIC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC 324CN Linear Low Density Polyethylene for Wire & Cable.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: 324CN is a Linear Low Density Polyethylene natural resin for wire and cable applications. It contains a low level of antioxidants and does not contain any slip or antiblock additives. Sufficient antioxidant and Cu-inhibitor should be added to meet specific ageing requirements. For jacketing applications, addition of Carbon Black or UV stabilizer is required.Typical Applications: One-step or two-step Silane cross-linkable insulation for Low Voltage power insulation cable, Aerial bundle cable, also suitable for telecommunication and Low Voltage power cable jacketing.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
load density; ASTM D1505
Melt Flow 3.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ASTM D2240
Tensile Strength at Break 18.0 MPa
2610 psi
ASTM D638
Tensile Strength, Yield 11.0 MPa
1600 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Elongation at Yield 14 %
14 %
ASTM D638
1% Secant Modulus 225 MPa
32600 psi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 121 °C
250 °F
Peak; SABIC Method
Electrical Properties Metric English Comments
Volume Resistivity 1.40e+18 ohm-cm
1.40e+18 ohm-cm
at 500 V; ASTM D257
Dielectric Constant 2.28

@Frequency 1000 Hz
2.28

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 37.0 kV/mm
940 kV/in
1000 V/sec; ASTM D149
Dissipation Factor 0.00043

@Frequency 1000 Hz
0.00043

@Frequency 1000 Hz
ASTM D150