Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 121 °C | 250 °F | Peak; SABIC Method |
SABIC 324CN Linear Low Density Polyethylene for Wire & Cable Product Description: 324CN is a Linear Low Density Polyethylene natural resin for wire and cable applications. It contains a low level of antioxidants and does not contain any slip or antiblock a.. |
|||
Melting Point | 121 °C | 250 °F | Internal method |
Polimeri Europa Flexirene® FG 23 I Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 I represents the version of Flexirene FG 20 I.. |
|||
Melting Point | 121 °C | 250 °F | Internal method |
Polimeri Europa Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene Flexirene CL 10 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexire.. |
|||
Melting Point | 121 °C | 250 °F | Internal method |
Polimeri Europa Flexirene® FG 23 F Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 F is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 F represents the version of Flexirene FG 20 F.. |
|||
Melting Point | 121 °C | 250 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 41E532 Anhydride-Modified LLDPE Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melting Point | 121 °C | 250 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Exceed™ 1023CA Tough Premium Film Resin
(discontinued **) Exceed 1023CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023CA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Melting Point | 121 °C | 250 °F | Exxon Method |
ExxonMobil Exceed™ 399L60 LDPE/Hexene Premium Blown Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 399L60 resin have balanced tensile, impact strength,.. |
|||
Melting Point | 121 °C | 250 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5028 400 Micron LLDPE Powder Description: ICOFLO 510-5028 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 121 °C | 250 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5073 500 Micron LLDPE Powder Description: ICOFLO 510-5073 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 121 °C | 250 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5074 800 Micron LLDPE Powder Description: ICOFLO 510-5074 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 121 °C | 250 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5075 1200 Micron LLDPE Powder Description: ICOFLO 510-5075 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 121 - 130 °C | 250 - 266 °F | |
Indium Corp. Indalloy 70 Indium-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 121 - 136 °C | 250 - 277 °F | |
Indium Corp. Indalloy 79 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 121 °C | 250 °F | ASTM D2117 |
Lushan M-10D Adhesive Resin for Multi-layer Sausage Casing film Adhesive resin Lushan series for sausages casing film is anhydride-modified polyethylene product and is available in pellet form. Adhesive resin Lushan series for sausages casing film is designed fo.. |
|||
Melting Point | 121 °C | 250 °F | ASTM D2117 |
Lushan M-10H Adhesive Resin for Multi-layer Sausage Casing film Adhesive resin Lushan series for sausages casing film is anhydride-modified polyethylene product and is available in pellet form. Adhesive resin Lushan series for sausages casing film is designed fo.. |
|||
Melting Point | >= 121 °C | >= 250 °F | ISO 3146 |
Borealis Borcoat™ ME0433 Polyethylene Adhesive In Powder form for Steel Pipe Coating Borcoat ME0433 is a maleic-anhydride grafted polyethylene polymer with excellent adhesion to fusion bonded epoxy and the top-coat HDPE.Borcoat HE0433 is primarily designed to be used as the tie laye.. |
|||
Melting Point | 121 °C | 250 °F | ISO 11357-3 |
Borealis FG5199 Linear Low Density Polyethylene FG5199 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-Fog and cling additives. The grade is developed for blown cling film. Film made from FG5199 is suit.. |
|||
Melting Point | 121 °C | 250 °F | ISO 11357 |
Total LLDPE LL 1820 H Linear Low Density Polyethylene - Blown Film LL 1820 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 H can be processed at high o.. |
|||
Melting Point | 121 °C | 250 °F | Crystalline; ISO 11357 |
Total Lotrene® Q2018C Linear Low Density Polyethylene, Blown Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Melting Point | 121 °C | 250 °F | Crystalline; ISO 11357 |
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Melting Point | 121 °C | 250 °F | Crystalline; ISO 11357 |
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Melting Point | 121 °C | 250 °F | ISO 11357 |
Total Lumicene® mPE M 2704 EP S01 Metallocene Polyethylene, Blown Film This product is a Total Ecosolutions grade.Lumicene® mPE M 2704 EP S01 is a second generation metallocene based Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2704 EP S01 can be.. |
|||
Melting Point | 121 °C | 250 °F | ASTM D3418, ISO 3146 |
DuPont™ Bynel® 4140 Anhydride Modified LLDPE BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melting Point | 121 °C | 250 °F | ASTM D3418, ISO 3146 |
DuPont™ Bynel® 41E871 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Melting Point | 121 °C | 250 °F | Dow Method (DSC) |
Dow DOWLEX™ 2056G Linear Low Density Polyethylene Improved thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Melting Point | 121 °C | 250 °F | Dow Method (DSC) |
Dow DOWLEX™ 2085G Polyethylene Resin DOWLEX™ 2085G is an ethylene-octene copolymer designed for general purpose thin gauge film applications. It is perfect for high strength consumer trash bags/liners. This product can be used in ot.. |
|||
Melting Point | 121 °C | 250 °F | ASTM D3418, ISO 3146 |
DuPont™ Bynel® 41E766 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Melting Point | 121 °C | 250 °F | DSC |
Arkema Group OREVAC® 18345 RNP Pipe Coating Binder Resin OREVAC 18345 RNP is a range of modified polyethylene which, when molten, have excellent adhesive properties to various substrates and are designed to bond dissimilar materials. It is supplied in bla.. |
|||
Melting Point | 121 °C | 250 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 41E558 Anhydride-Modified LLDPE Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |