Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.40e+18 ohm-cm | 1.40e+18 ohm-cm | at 500 V; ASTM D257 |
SABIC 324CN Linear Low Density Polyethylene for Wire & Cable Product Description: 324CN is a Linear Low Density Polyethylene natural resin for wire and cable applications. It contains a low level of antioxidants and does not contain any slip or antiblock a.. |