Polymer Property : Izod Impact, Notched = 2.35 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.35 J/cm
4.40 ft-lb/in
73°F; ASTM D256
Ravago Manufacturing Americas Hylon® N2033HL Nylon 6 (Cond)
Information provided by Ravago.
Izod Impact, Notched 2.35 J/cm
4.40 ft-lb/in
ASTM D256
Rotuba MH Cellulose Acetate
Property values at 50% RH.Data provided by the manufacturer.
Izod Impact, Notched 2.35 J/cm
4.41 ft-lb/in
ASTM D256 A
GRECO ISOPAK 547M ABS Resin
Metal Plating GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd.
Izod Impact, Notched 2.35 J/cm
4.40 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU
LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant.
Izod Impact, Notched 2.35 J/cm

@Thickness 6.35 mm
4.41 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® SD-0150U ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.35 J/cm

@Thickness 6.35 mm
4.41 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® SD-0150U ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.35 J/cm
4.40 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX951W PPE+PA66 (Asia Pacific)
A new high flow GTX designed for under-the-hood applications such as power distribution boxes, relay boxes and junction boxes. Developmental name: EXNX0151.
Izod Impact, Notched 2.35 J/cm
4.40 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PX1005X PPE+HIPS (Asia Pacific)
PPE+PS 80deg.C FR V-0
Izod Impact, Notched 2.35 J/cm

@Thickness 3.17 mm
4.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6/6 LGF60 HS L BK 12 mm
Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant, UV Stabilized and Heat StabilizerFeatures: Lubricated and Heat StabilizedProcessing Method: Inject..
Izod Impact, Notched 2.35 J/cm

@Temperature 23.0 °C
4.40 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl EBN3001 PPE+HIPS (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 2.35 J/cm
4.40 ft-lb/in
32°F; ASTM D256A
Dow TF0807 TPO
Dow Fascia TPO for Painted ApplicationsInformation provided by Dow
Izod Impact, Notched 2.35 J/cm
4.41 ft-lb/in
ASTM D256
E-Polymers TEKAMID® TB110SG30 30% Glass Fiber Reinforced, High Impact PA6 Resin
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,..
Izod Impact, Notched 2.35 J/cm

@Thickness 3.17 mm
4.40 ft-lb/in

@Thickness 0.125 in
ASTM Test
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
Izod Impact, Notched 2.35 J/cm
4.40 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL EX130 PPE+HIPS (Asia Pacific)
PPE+PS Auto Exterior Grade