Polymer Property : Tensile Strength, Ultimate = 5220 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ISO 527-2
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ASTM D638
Rotuba MH Cellulose Acetate
Property values at 50% RH.Data provided by the manufacturer.
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ASTM D638
Ineos Nova Zylar® 220 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features:High clarity Good elongation Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class VI plasticsApplications:D..
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ASTM D638
Global G-2855 High Density Polyethylene, Blow Molding Grade  (discontinued **)
Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- auto parts, bottles, housewares, drums, containers, bottlesMeets FDA requirements as listed in..
Tensile Strength, Ultimate 36.0 - 55.7 MPa
5220 - 8080 psi
Average value: 48.6 MPa Grade Count:7
Overview of materials for Phenolic, Novolac, Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o..
Tensile Strength, Ultimate 36.0 - 140 MPa
5220 - 20300 psi
Average value: 80.4 MPa Grade Count:7
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu..
Tensile Strength, Ultimate 36.0 MPa

@Temperature 22.0 °C
5220 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Menzolit Menzolit® BMC 0390 Unsaturated Polyester UP
BMC 0390 is a low profile DMC/BMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surface qua..
Tensile Strength, Ultimate 36.0 MPa

@Temperature 22.0 °C
5220 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Menzolit Menzolit® BMC 0400 Unsaturated Polyester UP
BMC 0400 is a low profile DMC/BMC for automotive applications. It fulfills the requirements of the automotive industry regarding painted body panels including reduced C-emissions. For highest surfac..
Tensile Strength, Ultimate 36.0 MPa

@Temperature 22.0 °C
5220 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Menzolit Menzolit® BMC 1000 Unsaturated Polyester UP
BMC 1000 is a special BMC for hydrolysis resistant applications. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Typical applic..
Tensile Strength, Ultimate 36.0 MPa
5220 psi
Type 1, 2"/min; ASTM D638
Stratasys® ABSplus
ABSplus is up to 40 percent stronger than standard ABS material and is an ideal material for conceptual prototyping through design verification through direct digital manufacturing. The marriage of ..
Tensile Strength, Ultimate 36.0 MPa
5220 psi
Type 1, 2"/min; ASTM D638
Stratasys® ABS-M30
ABS-M30 is 25-70 percent stronger than standard Stratasys ABS and is an ideal material for conceptual prototyping, design verification, and direct digital manufacturing. ABS-M30 has greater tensile,..
Tensile Strength, Ultimate 36.0 MPa
5220 psi
DIN 53504
Lubrizol ESTANE® T5134 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tensile Strength, Ultimate 36.0 MPa
5220 psi
DIN 53504
Lubrizol ESTANE® T5384 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ASTM D638
Lubrizol Isoplast® 301 Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ISO 527-1
Chengdu Polyster H605B Thermoplastic Polyether-ester Elastomer (TPEE)
Medium modulus molding and extrusion grade. Contains color-stable antioxidants. Good balance of low and high temperature properties. Good melt stability. CVJ boots, dust cover, bellows, jackets and ..
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ISO 527-1
Chengdu Polyster H7560 Thermoplastic Polyether-ester Elastomer (TPEE)
High modulus molding and injection grade. Contains improved color- stable antioxidants. Good balance of modulus and toughness. Parts and components of automobile, wires, cables and optical fiber, ho..
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ISO 527-1
Chengdu Polyster H7560Y Thermoplastic Polyether-ester Elastomer (TPEE)
High modulus molding and extrusion grade. Contains improved color- stable antioxidants. Low frictional coefficient and good abrasion resistance. Spherical socket of ball joint and lock of automobile..
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ASTM D412
BASF Elastollan® C-80A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen..
Tensile Strength, Ultimate 36.0 MPa
5220 psi
Z direction; ASTM D638
ALM PA 250 Nylon 12 SLS Prototyping Polymer
Highly Recyclable Nylon 12 Laser Sintering Material.Engineered for excellent mechanical properties, part definition and surface finish. Stabilized against thermal degradation resulting in little or..
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ASTM D638
A. Schulman ComAlloy Comtuf® 618 Nylon 6, Mineral Reinforced, Impact Modified
Data provided by the manufacturer, ComAlloy International Company.15% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i..
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ASTM D412
BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes...
Tensile Strength, Ultimate 36.0 MPa
5220 psi
DIN 53504
Lubrizol ESTANE® ETE60DT3 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ASTM D638
Plenco 7321 Phenolic, Nodular, Injection Molded
PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon..
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ISO 527-1/-2
DSM Arnitel® CM622 TPC-ES
60 Shore D, Extrusion
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ISO 37
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tensile Strength, Ultimate 36.0 - 45.0 MPa
5220 - 6530 psi
ISO 527
BASF Ecoflex® C1200 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2332 is our biodegradable, statistical, aliphatic-aromatic copolyester based on the monomers 1,4-butanediol, adipic acid and terephathalic acid in the polymer chain. E..