Material Notes:
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to match a variety of specific application parameters, including MIL-APPROVED. Custom designed bonding products and expert technical assistance are always available.Resin Technology Group 160-EX Oxy-Bond™ Two-Component Epoxy AdhesiveHigh performance, toughened, general purpose adhesive.
Physical Properties Metric English Comments
Viscosity 60000 cP
60000 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
Pot Life 60 min
60 min
60 min
60 min