Material Notes:
Steel pipe coating High Density Polyethylene grade. Contains a minimum 2% of well dispersed carbon black.Characteristics:excellent weathering resistance, excellent processability, excellent adhesion. Information provided by Reliance Industries
Physical Properties Metric English Comments
Density 0.9534 g/cc
0.03444 lb/in³
ASTM D1505
Water Absorption <= 0.050 %
<= 0.050 %
at 23°C/50°C; ASTM D570
Environmental Stress Crack Resistance >= 400 hour
>= 400 hour
F<sub>50</sub>; ASTM D1693
Oxidative Induction Time (OIT) >= 65 min
>= 65 min
ASTM D3895
Melt Flow 0.265 g/10 min

@Load 2.16 kg
0.265 g/10 min

@Load 4.76 lb
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength at Break 27.0 MPa
3920 psi
ASTM D638
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.730 GPa
106 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 122 °C
252 °F
ASTM D1525
Brittleness Temperature -75.0 °C
-103 °F
ASTM D746
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 2.4
2.4
ASTM D1531
Dielectric Strength >= 30.0 kV/mm
>= 762 kV/in
100 volt/sec; ASTM D149
Dissipation Factor 0.00050
0.00050
ASTM D1531