Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos 3560 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos 3560 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a special high melt flow, nucleated, high impact copolymer polypropylene for injection molding applications. It offers excellent impact resistance and a high flexural modulus.ApplicationsAutomotiveConsumer productsIndustrial applicationsBenefitsHigh impact resistanceHigh flexural modulusInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 49
49
ASTM D785
Tensile Strength, Yield 20.0 MPa

@Temperature 23.0 °C
2900 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Break 80 %
80 %
ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
D790B
Izod Impact, Notched 0.908 J/cm

@Temperature -20.0 °C
1.70 ft-lb/in

@Temperature -4.00 °F
1/8'' notched bar; ASTM D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
1/8'' notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
215 °F
ASTM D648
Descriptive Properties Value Comments
Multi-axial Instrumented Impact (10.9 ft/s) 13.2
negative 20°C, energy at max load, D3763
ductile
failure mode, D3763
Users viewing this material also viewed the following: