Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.265 - 34.0 g/10 min | 0.265 - 34.0 g/10 min | Average value: 9.85 g/10 min Grade Count:9 |
Overview of materials for High Density Polyethylene (HDPE), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Carbon Black Filled". Each property range of values reported is minimu.. |
|||
Melt Flow | 0.265 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.265 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
LyondellBasell Lupolen® 5021 D HDPE, Blow Molding Grade Easy flow, blow molding grade for small containers (up to 5 l), bottles for surface-active substances, household chemicals, laundry and dishwashing detergents, sanitary cleaners, cosmetics and pharm.. |
|||
Melt Flow | 0.265 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.265 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
LyondellBasell Lupolen® 5621 D HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melt Flow | 0.265 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.265 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
LyondellBasell Lupolen® 6021 D HDPE, Blow Molding Grade Easy flow, blow molding grade for small, rigid, thin-walled containers (up to 5 l), pots (up to 1 l), bottles and canisters (up to 5 l) for packaging mineral oil, antifreeze, brake fluid; drink bott.. |
|||
Melt Flow | 0.265 g/10 min @Load 2.16 kg |
0.265 g/10 min @Load 4.76 lb |
ASTM D1238 |
Reliance Industries Relene C31101 Polyethylene Steel pipe coating High Density Polyethylene grade. Contains a minimum 2% of well dispersed carbon black.Characteristics:excellent weathering resistance, excellent processability, excellent adhesio.. |