Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylon® N1035HLHR Nylon 6/6 (DAM)  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N1035HLHR Nylon 6/6 (DAM)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Ravago.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
0.125 in; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 193 MPa
28000 psi
73°F; ASTM D638
Elongation at Break 2.0 %
2.0 %
73°F; ASTM D638
Flexural Strength 241 MPa
35000 psi
73°F; ASTM D790
Flexural Modulus 9.31 GPa
1350 ksi
73°F; ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 249 °C
480 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Holding Pressure 750 to 1400 psi
Injection Rate Fast