Material Notes:
Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths. ## in the product number indicates roll length in yards. RB tape is designed for high instantaneous adhesion when brought into contact under light pressure.Design/Construction:Rubber: Cured Self-Fusing Silicone RubberCross-Section: 1” Wide Triangular Interleave: PolyethyleneThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Arlon SQA-TMS-024
Water Absorption 1.0 %
1.0 %
Arlon SQA-TMS-016
Thickness 1020 microns
40.0 mil
Rubber; Arlon SQA-TMS-012
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength 10.0 MPa
1450 psi
ASTM D412
Elongation at Break 473 %
473 %
ASTM D412
Peel Strength 0.543 kN/m
3.10 pli
Bond Strength; Arlon SQA-TMS-015
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 20.6 kV/mm
522 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red