Ravago Manufacturing Americas Enviramid™ N2300HL BK Post Consumer Recycle Nylon 6

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Enviramid™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Enviramid™ N2300HL BK Post Consumer Recycle Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat Stabilized, Lubricated, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Water Absorption 1.6 %
1.6 %
Saturation, Immersed; ASTM D570
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm

@Thickness 3.17 mm
0.015 - 0.019 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Flexural Strength 114 MPa
16500 psi
ASTM D790
Flexural Modulus 2.800 GPa
406.1 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
ASTM D648