Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Echo® RPH20TC BK Recycled Polypropylene Homopolymer, 20% Talc Filled

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Echo®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Echo® RPH20TC BK Recycled Polypropylene Homopolymer, 20% Talc Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Post Consumer Homopolymer Propylene (Nylon content < 5%), 12 Melt Flow, 20% Talc Filled, Heat Stabilized, BlackInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ISO 1183
Melt Flow 8.0 - 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 - 16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Ash 16 - 24 %
16 - 24 %
ISO 3451
Mechanical Properties Metric English Comments
Tensile Strength 24.0 MPa
3480 psi
ISO 527
Flexural Modulus 2.00 GPa
290 ksi
ISO 178
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO 179-1