Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 24.0 MPa | 3480 psi | ASTM D638 |
Metabolix Mirel™ F1006 Injection Molding Grade PHA Bioplastic Mirel F1006 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such.. |
|||
Tensile Strength | 24.0 MPa | 3480 psi | ISO 37 |
Kraton® D1186 A (SBS) Branched Block Copolymer Description: Kraton D1186 A is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows.. |
|||
Tensile Strength | 24.0 MPa | 3480 psi | Measured on films cast from a solution in toluene; ISO 37 |
Kraton® D1186 B (SBS) Branched Triblock Copolymer Description: Kraton D1186 BT is a clear, branched triblock copolymer based on styrene and butadiene with a polystyrene content of 30%. It is supplied from South America in the physical form identifi.. |
|||
Tensile Strength | 24.0 MPa | 3480 psi | ISO 37 |
Kraton® D1186 E (SBS) Branched Block Copolymer Description: Kraton D1186 E is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows.. |
|||
Tensile Strength | >= 24.0 MPa | >= 3480 psi | molded; ASTM D4894 |
Guarniflon PTFE G400 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |
|||
Tensile Strength | >= 24.0 MPa | >= 3480 psi | extruded; ASTM D4894 |
Guarniflon PTFE G500 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |
|||
Tensile Strength | >= 24.0 MPa | >= 3480 psi | extruded; ASTM D4894 |
Guarniflon PTFE G800 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |
|||
Tensile Strength | 24.0 MPa | 3480 psi | ASTM D638 |
Metabolix Mirelâ„¢ P1004 Injection Molding Grade PHA Bioplastic Mirel P1004 is a general purpose injection molding grade with high toughness.About Mirel BioplasticsMirel is a family of bioplastic materials that have physical properties comparable to petroleum-ba.. |
|||
Tensile Strength | 24.0 MPa | 3480 psi | DIN 53455 |
Isoflon PEHD 300 High Density Polyethylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Tensile Strength | >= 24.0 MPa | >= 3480 psi | Excellent |
Shandong Dongyue Polymer DF-201 PTFE Fine Powder Usage: It is suitable for making unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse.. |
|||
Tensile Strength | >= 24.0 MPa | >= 3480 psi | Excellent |
Shandong Dongyue Polymer DF-202 PTFE Fine Powder Usage: It is mainly used to process, belt, thin sheet and unsintered tape, thin wall rod etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTF.. |
|||
Tensile Strength | >= 24.0 MPa | >= 3480 psi | Grade A |
Shandong Dongyue Polymer DF-203 PTFE Fine Powder Usage: The resin is used to process capillary tube, thin-wall tube, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside... |
|||
Tensile Strength | >= 24.0 MPa | >= 3480 psi | Grade A |
Shandong Dongyue Polymer DF-204 PTFE Fine Powder Usage: The resin is mainly used for elastic tape, capillary tube, and the unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE s.. |
|||
Tensile Strength | >= 24.0 MPa | >= 3480 psi | Grade A |
Shandong Dongyue Polymer DF-205 PTFE Fine Powder Usage: The resin is used to process two-side draw film, capillary tube, thin-wall tube, sheet, small-diameter rod, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC ba.. |
|||
Tensile Strength | 24.0 - 31.0 MPa | 3480 - 4500 psi | DIN 53 455 |
Hippe PE 300 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Tensile Strength | 24.0 MPa @Strain 5.00 %, Temperature 60.0 °C |
3480 psi @Strain 5.00 %, Temperature 140 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 1000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 24.0 MPa | 3480 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-2180 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 24.0 MPa | 3480 psi | ISO 527 |
Ravago Manufacturing Americas Echo® RPH20TC BK Recycled Polypropylene Homopolymer, 20% Talc Filled Post Consumer Homopolymer Propylene (Nylon content < 5%), 12 Melt Flow, 20% Talc Filled, Heat Stabilized, BlackInformation provided by Ravago. |