Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 12 - 16 g/10 min | 12 - 16 g/10 min | ASTM D1238 |
S&E Specialty Polymers GPP™ 1005M-EXLT PP Application: UL94 V-2, Non-blooming flame retardant polypropylene compound for injection molding.Information provided by S&E Specialty Polymers |
|||
Melt Flow | 4.0 - 16 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.0 - 16 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and.. |
|||
Melt Flow | 4.0 - 16 g/10 min | 4.0 - 16 g/10 min | ASTM D1238 |
Polymer Resources ABS-FR1 ABS, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 14 - 16 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 - 16 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-FD2-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted.. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Melt Flow | 8.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-UV2-D-[color]-1 Polycarbonate, UV-stabilized, Medium Flow with Mold Release Polycarbonate, UV-stabilized, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Melt Flow | 8.0 - 16 g/10 min @Load 2.16 kg, Temperature 250 °C |
8.0 - 16 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources TP-G15 Polybutylene Terephthalate, 15% Glass Reinforced Polybutylene Terephthalate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Melt Flow | 8.0 - 16 g/10 min @Load 2.16 kg, Temperature 250 °C |
8.0 - 16 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources TP-IM-G15 Polybutylene Terephthalate, 15% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 15% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Melt Flow | 8.0 - 16 g/10 min @Load 2.16 kg, Temperature 250 °C |
8.0 - 16 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources TP-IM-G7.5 Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Melt Flow | 10 - 16 g/10 min | 10 - 16 g/10 min | ASTM D1238-92 |
Iran Petrochemical (PCC) Tabriz 6630/1 High Impact Polystyrene
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Melt Flow | 8.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-HM-FR2-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Melt Flow | 10 - 16 g/10 min @Load 2.16 kg, Temperature 250 °C |
10 - 16 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
GRECO ISOPAK 625 Polycarbonate/ABS Alloy General purpose polycarbonate/ABS alloy; good impact and dimensional stabilityInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Melt Flow | 12 - 16 g/10 min | 12 - 16 g/10 min | Cond L; ASTM D1238 |
Washington Penn PPH5CF5 Polypropylene, 50% Calcium Carbonate Filled UV Stabilized; Injection molding grade.Applications: Commonly used as a concentrate. High flow for thin wall parts requiring long-flow. Toys, small appliances, outdoor furniture.Data provided by W.. |
|||
Melt Flow | 8.0 - 16 g/10 min | 8.0 - 16 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 8.0 - 16 g/10 min | 8.0 - 16 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 8.0 - 16 g/10 min | 8.0 - 16 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 8.0 - 16 g/10 min | 8.0 - 16 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 10 - 16 g/10 min | 10 - 16 g/10 min | ASTM D1238 |
Buckeye Polymers BP RPP 4010 T NAT Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |
|||
Melt Flow | 10 - 16 g/10 min | 10 - 16 g/10 min | ASTM D1238 |
Buckeye Polymers BP RPPC 1813 C BLK Polypropylene, Calcium Filled Product Information: Calcium Carbonate Filled PP Grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. Our BP RPP C series product line ranges fro.. |
|||
Melt Flow | 10 - 16 g/10 min | 10 - 16 g/10 min | ASTM D1238 |
Buckeye Polymers BP RPP 2012 TR BLK Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |
|||
Melt Flow | 14 - 16 g/10 min | 14 - 16 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 6421 BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 14 - 16 g/10 min | 14 - 16 g/10 min | ASTM D1238 |
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 8.0 - 16 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 - 16 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 - ISO 1133 |
DuPont Elvaloy® HP663 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer
(discontinued **) Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |