Mechanical Properties Metric English Comments
Tensile Strength 24.0 MPa
3480 psi
ASTM D638
Metabolix Mirelâ„¢ F1006 Injection Molding Grade PHA Bioplastic
Mirel F1006 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such..
Tensile Strength 24.0 MPa
3480 psi
ISO 37
Kraton® D1186 A (SBS) Branched Block Copolymer
Description: Kraton D1186 A is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows..
Tensile Strength 24.0 MPa
3480 psi
Measured on films cast from a solution in toluene; ISO 37
Kraton® D1186 B (SBS) Branched Triblock Copolymer
Description: Kraton D1186 BT is a clear, branched triblock copolymer based on styrene and butadiene with a polystyrene content of 30%. It is supplied from South America in the physical form identifi..
Tensile Strength 24.0 MPa
3480 psi
ISO 37
Kraton® D1186 E (SBS) Branched Block Copolymer
Description: Kraton D1186 E is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows..
Tensile Strength >= 24.0 MPa
>= 3480 psi
molded; ASTM D4894
Guarniflon PTFE G400 Polytetrafluoroethylene
A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif..
Tensile Strength >= 24.0 MPa
>= 3480 psi
extruded; ASTM D4894
Guarniflon PTFE G500 Polytetrafluoroethylene
A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif..
Tensile Strength >= 24.0 MPa
>= 3480 psi
extruded; ASTM D4894
Guarniflon PTFE G800 Polytetrafluoroethylene
A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif..
Tensile Strength 24.0 MPa
3480 psi
ASTM D638
Metabolix Mirelâ„¢ P1004 Injection Molding Grade PHA Bioplastic
Mirel P1004 is a general purpose injection molding grade with high toughness.About Mirel BioplasticsMirel is a family of bioplastic materials that have physical properties comparable to petroleum-ba..
Tensile Strength 24.0 MPa
3480 psi
DIN 53455
Isoflon PEHD 300 High Density Polyethylene
Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon.
Tensile Strength >= 24.0 MPa
>= 3480 psi
Excellent
Shandong Dongyue Polymer DF-201 PTFE Fine Powder
Usage: It is suitable for making unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse..
Tensile Strength >= 24.0 MPa
>= 3480 psi
Excellent
Shandong Dongyue Polymer DF-202 PTFE Fine Powder
Usage: It is mainly used to process, belt, thin sheet and unsintered tape, thin wall rod etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTF..
Tensile Strength >= 24.0 MPa
>= 3480 psi
Grade A
Shandong Dongyue Polymer DF-203 PTFE Fine Powder
Usage: The resin is used to process capillary tube, thin-wall tube, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside...
Tensile Strength >= 24.0 MPa
>= 3480 psi
Grade A
Shandong Dongyue Polymer DF-204 PTFE Fine Powder
Usage: The resin is mainly used for elastic tape, capillary tube, and the unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE s..
Tensile Strength >= 24.0 MPa
>= 3480 psi
Grade A
Shandong Dongyue Polymer DF-205 PTFE Fine Powder
Usage: The resin is used to process two-side draw film, capillary tube, thin-wall tube, sheet, small-diameter rod, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC ba..
Tensile Strength 24.0 - 31.0 MPa
3480 - 4500 psi
DIN 53 455
Hippe PE 300 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
Tensile Strength 24.0 MPa

@Strain 5.00 %,
Temperature 60.0 °C
3480 psi

@Strain 5.00 %,
Temperature 140 °F
50 mm/min; ISO 527-2
BASF Elastollan R 1000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength 24.0 MPa
3480 psi
ASTM D412
Wanhua Chemical Wanthane® WHT-2180 Polycaprolactone Based TPU
Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Tensile Strength 24.0 MPa
3480 psi
ISO 527
Ravago Manufacturing Americas Echo® RPH20TC BK Recycled Polypropylene Homopolymer, 20% Talc Filled