Radici Radilon® S ERV3808K (cond.) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® S ERV3808K (cond.) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Mechanical Properties Metric English Comments
Tensile Strength at Break 86.0 MPa
12500 psi
Elongation at Break 5.1 %
5.1 %
Tensile Modulus 5.70 GPa
827 ksi
Charpy Impact Unnotched 9.00 J/cm²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 3.20 J/cm²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 600 V
600 V
Users viewing this material also viewed the following: