Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® A RV250 (dry) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® A RV250 (dry) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
Water Absorption 7.4 %
7.4 %
Moisture Absorption at Equilibrium 2.0 %
2.0 %
Viscosity Measurement 145
145
cm³/g Viscosity Number
Mechanical Properties Metric English Comments
Tensile Strength at Break 160 MPa
23200 psi
Elongation at Break 3.6 %
3.6 %
Tensile Modulus 8.30 GPa
1200 ksi
Charpy Impact Unnotched 5.70 J/cm²

@Temperature -30.0 °C
27.1 ft-lb/in²

@Temperature -22.0 °F
6.10 J/cm²

@Temperature 23.0 °C
29.0 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.950 J/cm²

@Temperature -30.0 °C
4.52 ft-lb/in²

@Temperature -22.0 °F
1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
Vicat Softening Point 245 °C

@Load 5.10 kg
473 °F

@Load 11.2 lb
50°C/h
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved