Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Fluorosint® MT-01 PTFE + additives, enhanced grade, compression moulded (ISO Data)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Quadrant Engineering Plastics Products
Trade Name Fluorosint®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Fluorosint® MT-01 PTFE + additives, enhanced grade, compression moulded (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluorosint MT-01 is an extreme service grade developed specifically for applications where the benefits of PTFE-based materials also require strength, stiffness and stability. Fluorosint MT-01 delivers high mechanical performance at elevated temperature and as a result is often specified in seat, seal and wear applications where extreme conditions are present High maximum allowable service temperature in air (260°C continuously) Excellent chemical and hydrolysis resistance Outstanding UV- and weather resistance Physiologically inert (suitable for food contact, except Fluorosint 500, Fluorosint MT-01) Inherent low flammability Good electrical insulating properties
Physical Properties Metric English Comments
Density 2.27 g/cc
0.0820 lb/in³
ISO 1183-1
Water Absorption at Saturation 1.5 - 2.5 %
1.5 - 2.5 %
Mechanical Properties Metric English Comments
Hardness, Rockwell R 74
74
ISO 2039-2
Hardness, Shore D 70
70
Ball Indentation Hardness 55.0 MPa
7980 psi
ISO 2039-1
Tensile Strength 14.0 MPa
2030 psi
at Yield; ISO 527-1/-2
Elongation at Break 20 %
20 %
ISO 527-1/-2
Elongation at Yield 6.0 %
6.0 %
ISO 527-1/-2
Tensile Modulus 1.90 GPa
276 ksi
ISO 527-1/-2
Flexural Strength 20.0 MPa
2900 psi
Compressive Strength 11.0 MPa

@Strain 1 %
1600 psi

@Strain 1 %
ISO 604
17.0 MPa

@Strain 2 %
2470 psi

@Strain 2 %
ISO 604
29.0 MPa

@Strain 5 %
4210 psi

@Strain 5 %
ISO 604
K Factor (ISO) 6.0 µm/km
6.0 µm/km
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179-1/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.15 - 0.25
0.15 - 0.25
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C

@Temperature 23.0 - 100 °C
33.3 µin/in-°F

@Temperature 73.4 - 212 °F
Melting Point 327 °C
621 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 260 °C
500 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
Oxygen Index >= 95 %
>= 95 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 1e+05
<= 1e+05
IEC 60093
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Acceptable
Acceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Conductive / Static Dissipative Yes
Yes
Continuous Sunlight Acceptable
Acceptable
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Users viewing this material also viewed the following: