Proto3000 PC-ABS Fused Deposition Modeling Polymer

Category Polymer , Rapid Prototyping Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Proto3000
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Proto3000 PC-ABS Fused Deposition Modeling Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: PC-ABS (polycarbonate-ABS) is one of the most widely used industrial thermoplastics. PC-ABS offers the most desirable properties of both materials - the superior strength and heat resistance of PC and the ?exibility of ABS. PC-ABS blends are commonly used in automotive, electronics and telecommunications applications. Additionally, a PC-ABS part manufactured on a Fortus 3D Production System is 5-60 percent stronger than a part made on previous FDM systems. When combined with a Fortus system, PC-ABS gives you Real Parts™ conceptual modeling, functional prototyping, manufacturing tools, and end-use-parts.Available Colors: BlackInformation provided by Proto3000 for their protoyping engineering services.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength at Break 41.0 MPa
5950 psi
Type 1, 2"/min; ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
70 %
70 %
Flexural Elongation; ASTM D790
Tensile Modulus 1.917 GPa
278.0 ksi
ASTM D638
Flexural Strength 68.0 MPa
9860 psi
Method 1, 0.05"/min; ASTM D790
Flexural Modulus 1.931 GPa
280.1 ksi
ASTM D790
Izod Impact, Notched 1.96 J/cm
3.67 ft-lb/in
Method A; ASTM D256
Izod Impact, Unnotched 4.81 J/cm
9.01 ft-lb/in
Method A; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C

@Thickness 0.125 mm
230 °F

@Thickness 0.00492 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C

@Thickness 0.125 mm
205 °F

@Thickness 0.00492 in
ASTM D648
Vicat Softening Point 112 °C
234 °F
ASTM D1525
Glass Transition Temp, Tg 125 °C
257 °F
DAM (SSYS)
Flammability, UL94 HB

@Thickness 0.850 mm
HB

@Thickness 0.0335 in
Electrical Properties Metric English Comments
Dielectric Constant 3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
IEC 60250
3.1

@Frequency 100 Hz
3.1

@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60112