Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.931 GPa | 280.1 ksi | ASTM D790-1 |
Ineos Styrenics Avantra® 525K High Impact Styrenic Polymer (NAFTA) Description: Specialty and super-high impact grades for a variety of applications such as refrigerator liners, consumer electronics housings, recreation equipment and sporting goods, toys, office pr.. |
|||
Flexural Modulus | 1.931 GPa | 280.1 ksi | ASTM D790 |
Lucent Polymers CPP-120 Polypropylene Homopolymer, 20% Calcium Carbonate Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 1.931 GPa | 280.1 ksi | ASTM D790 |
Eastman Tenite Acetate 105E1R26033 Clear, Trsp Cellulose Acetate Plasticizer 29%. Weight loss on heating = 2.6% per ASTM D 707. Soluble matter loss = 0.4% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.931 GPa | 280.1 ksi | ASTM D790 |
Proto3000 PC-ABS Fused Deposition Modeling Polymer Description: PC-ABS (polycarbonate-ABS) is one of the most widely used industrial thermoplastics. PC-ABS offers the most desirable properties of both materials - the superior strength and heat resis.. |