Protective Coating PC-7® Epoxy Paste

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Protective Coating Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Protective Coating PC-7® Epoxy Paste.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC-7® is a tough job Epoxy formulation developed for maximum bonding power. Components A (grey) and B (black), when mixed, react to form a bond of good strength. PC-7® formulation provides extended working time, giving user ample time to complete larger jobs, reposition work or make changes. High wet grab or tack of PC-7® makes overhead and sidewall work easy without drip or sag. PC-7® demonstrates excellent chemical resistance to mild acids, caustics, detergents, gasoline, fuel oil, salt, and fresh water. PC-7® will not bond to wax paper, TEFLON®, polyethylene, and some soft plastics.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Water Absorption 0.44 %
0.44 %
ASTM C413
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
1 Week Cure; ASTM D2240
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 20.0 MPa
2900 psi
ASTM D580
Compressive Yield Strength 29.0 MPa
4210 psi
ASTM D695
Adhesive Bond Strength 15.0 MPa
2180 psi
Tensile Shear Strength; ASTM D1002
Gardner Impact 18.0 J
13.3 ft-lb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C
120 °F
ASTM D648