LG Chemical PB900 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer LG Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical PB900 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General Description: PB900, homopolymer made by micro-suspension seeded polymerization, is PVC resin with pseudo plastic flow property. PB900 can be used for wall paper made by knife coating/rotary screen coating.Main Applications: Wall coveringsCAS No: 9002-86-2Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.406 g/cc
1.406 g/cc
Bulk Density 0.300 - 0.400 g/cc
0.0108 - 0.0145 lb/in³
ASTM D1895
Volatiles <= 0.70 %

@Temperature 110 °C,
Time 3600 sec
<= 0.70 %

@Temperature 230 °F,
Time 1.00 hour
ASTM D3030-90
Brookfield Viscosity 3500 - 8500 cP
3500 - 8500 cP
DOP 60phr, 6RPM; ASTM D1824
Viscosity Measurement >= 2.0

@Pressure 0.400 MPa
>= 2.0

@Pressure 58.0 psi
[g/sec], DOP 60phr, Severs; ASTM D1823
Molecular Weight 60000 - 150000 g/mol
60000 - 150000 g/mol
Thermal Properties Metric English Comments
Melting Point 302 °C
576 °F
Descriptive Properties Value Comments
Autoignition Temperature 435°C
Degree of Polymerization 850-950
30°C, JIS K 6720-2
K-Value 64
DIN53726 / ISO1628-2