Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 3.0 µm | 3.0 µm | median; Microtrac |
Nyco NYAD® 5000 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Particle Size | >= 3.0 µm | >= 3.0 µm | 10% smaller than |
Nyco NYAD® MD325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Particle Size | >= 3.0 µm | >= 3.0 µm | 10% smaller than |
Nyco NYGLOS® MSTPO Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | >= 3.0 µm | >= 3.0 µm | 10% smaller than |
Nyco NYGLOS® STPO Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | 3.0 µm | 3.0 µm | Median Grain Diameter |
Nabaltec APYMAG® 80 Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Particle Size | <= 3.0 µm | <= 3.0 µm | Best Grade |
Oceanchem Group Decabromodiphenyl Ethane (DBDPE/8010) Molecular Formula: C14Br10H4Cas No.: 84852-53-9Characteristics: White powder, no poison, no smell and noncorrosion. Indissolvable in water, ethyl alcohol, acetone, benzene, arene chloride.Use: This.. |
|||
Particle Size | <= 3.0 µm | <= 3.0 µm | Best Grade |
Oceanchem Group Decabromodiphenyl Oxide (DECA/DBDPO) Molecular Formula: C12Br10OCas No.: 1163-19-5Characteristics: White powder, no poison, no smell and noncorrosion. Indissolvable in water, ethyl alcohol, acetone, benzene, arene chloride.Use: It is .. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | First Grade |
Oceanchem Group Zinc Borate Information Provided by Oceanchem Group |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles |
Ferro EG 0024 Specialty Glass Glass Type: Si-B-MG-Al Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-ph.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles |
Ferro EG 2782 Specialty Glass Glass Type: Ca-Si-B Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-phase.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles, (RWG Powder) |
Ferro IP 750 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles, (RWG Powder) |
Ferro IP 760 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 3.0 - 4.5 µm | 3.0 - 4.5 µm | d50 |
Magyar Aluminum ALO-EL-3S Alumina Ground Alumina |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | d50 |
Magyar Aluminum Zeolite |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | average |
Malvern Minerals Novakup® L-207A Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 3.0 µm | 3.0 µm | Crystal Size |
Momentive Performance Materials HCPH Boron Nitride (BN) Powder GE Advanced Ceramics boron nitride (BN) powders of grades HCP, HCPH, HCPL, and AC6004 are generally single-crystal hexagonal platelets with very high purity. The mean particle sizes for these ultra-.. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade A Zirconium Diboride, ZrB2 Hot-pressed composites of excellent electrical conductivity, e.g., evaporation boats for continuous aluminum metallizingCrucible material for non-ferrous metalsCeramic shapes to be used in productio.. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | Laser Diffraction D50 |
H.C. Starck Grade B Zirconium Carbide, ZrC Additive for hard metalsAdditive for powder metallurgyModerator in solid fuel propellant |
|||
Particle Size | 3.0 - 6.0 µm | 3.0 - 6.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade SE Titanium Diboride, TiB2 Higher N, O, Fe contentsHot-pressed composites of excellent electrical conductivity, e.g., evaporation boats for continuous aluminum metallizingCrucible material for non-ferrous metalsCeramic shapes.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles |
Ferro EG 0002 Glazes and Sealants Glass Type: Si-Al-Ba Typical Powder Form: VWG Typical Application: SiC Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulatin.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles, (RWG Powder) |
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles, (RWG Powder) |
Ferro IP 770 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | Median Grain (d50) |
CeramTec Rubalit® 708S Alumina, 96% Rubalit® 708S (96%) is an alumina that features high strength and thermal conductivity. It provides outstanding results when used on commercially available thick-film pastes and metallization syste.. |
|||
Particle Size | 3.0 - 4.0 µm | 3.0 - 4.0 µm | |
Dow Corning PF-2520 ELASTOMER EMULSION DOW CORNING® PF-2520 Elastomer Emulsion has been developed to facilitate the incorporation of an elastomeric powder in fluid into water-based silicone powder into water-based cosmetic products. It .. |
|||
Particle Size | 3.0 µm | 3.0 µm | D50 |
Dandong Taico Minerals TAICOCITE® TC35 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Particle Size | 3.0 µm | 3.0 µm | Median |
CIMBAR CIMBAR™ XF Barite Powder (BaSO4) CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical .. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50" Percentile |
3M W-210 Ceramic Microspheres 3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l.. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | Medium Grain (d50) |
CeramTec Rubalit® 708 HP Alumina, 96% (High Performance) Rubalit® 708 HP (High Performance) has been developed from Rubalit® 708S. This material shares the same chemical composition, is produced on the same plant and using the identical production techn.. |
|||
Particle Size | >= 3.0 µm | >= 3.0 µm | D10 |
Potters Industries A-Series Z-CEL® 8054 White Synthetic Sodium Aluminosilicate Microsphere Fine particle white spheres developed as filler for paints, coatings and films.Information provided by Potters Industries. |