Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamSter PE304G3 PET, 15% Glass Fiber

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 20% Glass Reinforced
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamSter PE304G3 PET, 15% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
15% Glass fiber reinforced, heat stabilized and impact modified PET for injection molding application.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.25 %
0.25 %
50% RH; ISO 62
Linear Mold Shrinkage 0.0015 - 0.0030 cm/cm
0.0015 - 0.0030 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
ISO 527
Elongation at Break 4.0 %
4.0 %
ISO 527
Tensile Modulus 4.50 GPa
653 ksi
ISO 527
Flexural Modulus 4.00 GPa
580 ksi
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 187 °C
369 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Users viewing this material also viewed the following: