Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram PlusTek RA321G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant
Manufacturer Polyram
Trade Name PlusTek
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek RA321G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
DIN 53479
Water Absorption 4.5 %
4.5 %
DIN 53495
Moisture Absorption at Equilibrium 1.5 %
1.5 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 140 MPa
>= 20300 psi
ASTM-D638
Elongation at Break 2.0 %
2.0 %
ASTM-D638
Flexural Strength >= 190 MPa
>= 27600 psi
ASTM D790
Flexural Modulus >= 7.50 GPa
>= 1090 ksi
ASTM-D790
Izod Impact, Notched >= 0.500 J/cm

@Temperature 23.0 °C
>= 0.937 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
Maximum Service Temperature, Air 115 °C
239 °F
Continuous Use
>= 200 °C
>= 392 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
DIN 53461
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
DIN 53482
Dielectric Constant 3.7

@Frequency 1e+6 Hz
3.7

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 80.0 kV/mm
2030 kV/in
VDE 0303/4