Polyram PlusTek RA300G6 Nylon 6.6, 30% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek RA300G6 Nylon 6.6, 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
DIN 53479
Water Absorption 0.80 %
0.80 %
DIN 53495
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 150 MPa
>= 21800 psi
ASTM-D638
Elongation at Break 3.0 %
3.0 %
ASTM-D638
Flexural Strength >= 210 MPa
>= 30500 psi
ASTM D790
Flexural Modulus >= 7.50 GPa
>= 1090 ksi
ASTM-D790
Izod Impact, Notched >= 0.750 J/cm

@Temperature 23.0 °C
>= 1.41 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
Deflection Temperature at 0.46 MPa (66 psi) >= 240 °C
>= 464 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) >= 210 °C
>= 410 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in