PolyOne Stat-Tech™ UR-7SS-5GF/000 PT GY Thermoplastic Elastomer - TPU, Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Stat-Tech™ UR-7SS-5GF/000 PT GY Thermoplastic Elastomer - TPU, Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Stainless Steel Fiber FilledGlass Fiber ReinforcedElectrically ConductiveInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 25.9 MPa
3750 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 0.8012 GPa
116.2 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus 0.579 GPa
84.0 ksi
ASTM D790
Izod Impact, Notched 0.908 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.70 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+6 ohm
1.00e+6 ohm
ASTM D257