Hannam Chemical Hanalac 711 ABS, Plating Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Plating Grade
Manufacturer Hannam Chemical
Trade Name Hanalac
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hannam Chemical Hanalac 711 ABS, Plating Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plating grade with excellent moldability and easy to surface treat. It also has a strong adhesive strength after plating and an excellent heat cycle. Applications: Appliances, TV frames, automotive parts, name plates.
Physical Properties Metric English Comments
Melt Flow 3.6 g/10 min
3.6 g/10 min
ASTM D1238G
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Ultimate 45.1 MPa
6540 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Yield Strength 56.0 MPa
8120 psi
ASTM D790
Flexural Modulus 2.16 GPa
313 ksi
ASTM D790
Izod Impact, Notched 2.90 J/cm

@Thickness 3.17 mm
5.43 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 85.0 °C
185 °F
Heat Distortion Temp
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Vicat Softening Point 96.0 °C
205 °F
ASTM D1525
Flammability, UL94 HB
HB