Oxford Polymers PBT 15GF-V0 UL Listed Polybutylene Terephthalate (PBT)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Unreinforced, Molded
Manufacturer Oxford Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers PBT 15GF-V0 UL Listed Polybutylene Terephthalate (PBT).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UL Listed Polybutylene Terephthalate (PBT)Information provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Modulus 4.65 GPa
675 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Temperature 23.0 °C
1.10 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
ASTM D648