Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.8012 GPa | 116.2 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Stat-Tech™ UR-7SS-5GF/000 PT GY Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **) Description/Features:Stainless Steel Fiber FilledGlass Fiber ReinforcedElectrically ConductiveInformation provided by PolyOne Corporation. |